Você está no 3DFinder
Buscamos em Thingiverse, MakerWorld e Printables ao mesmo tempo para te dar o melhor de cada uma.
Descrição
A little and fast Stringing and Bridging test that you can make in a few minutes and with low material wasted for it. I suggest to try to change this setting in order of importace:
- retraction mm (from 0.8 to 10)
- Speed of retraction (20 to 40mm/s)
- Try to lowering you themperature;
- Dry your filament;
- Buy better quality filament;
- Use z-hop (from 0.1mm to 0.4mm);
- Printing speed (fast in better).
- Fan (powerfull is better).
Others: Check nozzle usury, flow, step by mm etc...
First of all you need that your printer is calibrated.
Enjoy
8
Curtidas
0
Downloads
24
Coleções
Licença
Creative Commons - Attribution